Serveur d'exploration sur l'OCR

Attention, ce site est en cours de développement !
Attention, site généré par des moyens informatiques à partir de corpus bruts.
Les informations ne sont donc pas validées.

Instability map for cold and warm working of as-cast 304 stainless steel

Identifieur interne : 002403 ( Main/Exploration ); précédent : 002402; suivant : 002404

Instability map for cold and warm working of as-cast 304 stainless steel

Auteurs : S. Venugopal [Inde, États-Unis] ; S. L. Mannan [Inde] ; Y. V. R. K. Prasad [Inde]

Source :

RBID : ISTEX:040A787A1B603C71251632AF6F84F5D0445A9532

Abstract

The deformation characteristics of as-cast 304 stainless steel under compression in the temperature range 20–600 °C and strain rate range 0.001–100 s−1 have been studied with a view to characterizing the flow instabilities occurring in the microstructure. At strain rates of less than 0.05 s−1, as-cast 304 stainless steel exhibits flow localization in the temperature range 20–600 °C, whereas dynamic strain ageing occurs at intermediate temperatures and below 5 s−1. At room temperatures and strain rates of less than 0.05 s−1, martensite formation is observed. To avoid the above microstructural instabilities warm working should be carried out at strain rates greater than 10 s−1 in the temperature range 400–600 °C and cold working could be done in the range of about 0.05–0.8 s−1. The continuum criterion developed on the basis of the principles of maximum rate of entropy production and separability of the dissipation function, predicts accurately all of the above instability features.

Url:
DOI: 10.1016/0924-0136(95)02249-X


Affiliations:


Links toward previous steps (curation, corpus...)


Le document en format XML

<record>
<TEI wicri:istexFullTextTei="biblStruct">
<teiHeader>
<fileDesc>
<titleStmt>
<title>Instability map for cold and warm working of as-cast 304 stainless steel</title>
<author>
<name sortKey="Venugopal, S" sort="Venugopal, S" uniqKey="Venugopal S" first="S." last="Venugopal">S. Venugopal</name>
</author>
<author>
<name sortKey="Mannan, S L" sort="Mannan, S L" uniqKey="Mannan S" first="S. L." last="Mannan">S. L. Mannan</name>
</author>
<author>
<name sortKey="Prasad, Y V R K" sort="Prasad, Y V R K" uniqKey="Prasad Y" first="Y. V. R. K." last="Prasad">Y. V. R. K. Prasad</name>
</author>
</titleStmt>
<publicationStmt>
<idno type="wicri:source">ISTEX</idno>
<idno type="RBID">ISTEX:040A787A1B603C71251632AF6F84F5D0445A9532</idno>
<date when="1997" year="1997">1997</date>
<idno type="doi">10.1016/0924-0136(95)02249-X</idno>
<idno type="url">https://api.istex.fr/document/040A787A1B603C71251632AF6F84F5D0445A9532/fulltext/pdf</idno>
<idno type="wicri:Area/Istex/Corpus">003379</idno>
<idno type="wicri:Area/Istex/Curation">003125</idno>
<idno type="wicri:Area/Istex/Checkpoint">001853</idno>
<idno type="wicri:doubleKey">0924-0136:1997:Venugopal S:instability:map:for</idno>
<idno type="wicri:Area/Main/Merge">002533</idno>
<idno type="wicri:Area/Main/Curation">002403</idno>
<idno type="wicri:Area/Main/Exploration">002403</idno>
</publicationStmt>
<sourceDesc>
<biblStruct>
<analytic>
<title level="a">Instability map for cold and warm working of as-cast 304 stainless steel</title>
<author>
<name sortKey="Venugopal, S" sort="Venugopal, S" uniqKey="Venugopal S" first="S." last="Venugopal">S. Venugopal</name>
<affiliation wicri:level="1">
<country xml:lang="fr">Inde</country>
<wicri:regionArea>Materials Development Division, Indira Gandhi Centre for Atomic Research, Kalpakkam-603 102, Taml Nadu</wicri:regionArea>
<wicri:noRegion>Taml Nadu</wicri:noRegion>
</affiliation>
<affiliation wicri:level="2">
<country xml:lang="fr" wicri:curation="lc">États-Unis</country>
<wicri:regionArea>1 Presently as NRC Associate with Materials Process Design, Materials Directorate, Wright Laboratory, Wright Patterson Air Force Base, OH 45433-7746</wicri:regionArea>
<placeName>
<region type="state">Ohio</region>
</placeName>
</affiliation>
</author>
<author>
<name sortKey="Mannan, S L" sort="Mannan, S L" uniqKey="Mannan S" first="S. L." last="Mannan">S. L. Mannan</name>
<affiliation>
<wicri:noCountry code="no comma">Corresponding author.</wicri:noCountry>
</affiliation>
<affiliation wicri:level="1">
<country xml:lang="fr">Inde</country>
<wicri:regionArea>Materials Development Division, Indira Gandhi Centre for Atomic Research, Kalpakkam-603 102, Taml Nadu</wicri:regionArea>
<wicri:noRegion>Taml Nadu</wicri:noRegion>
</affiliation>
</author>
<author>
<name sortKey="Prasad, Y V R K" sort="Prasad, Y V R K" uniqKey="Prasad Y" first="Y. V. R. K." last="Prasad">Y. V. R. K. Prasad</name>
<affiliation wicri:level="1">
<country xml:lang="fr">Inde</country>
<wicri:regionArea>Department of Metallurgy, Indian Institute of Science, Bangalore-560 012</wicri:regionArea>
<wicri:noRegion>Bangalore-560 012</wicri:noRegion>
</affiliation>
</author>
</analytic>
<monogr></monogr>
<series>
<title level="j">Journal of Materials Processing Technology</title>
<title level="j" type="abbrev">PROTEC</title>
<idno type="ISSN">0924-0136</idno>
<imprint>
<publisher>ELSEVIER</publisher>
<date type="published" when="1995">1995</date>
<biblScope unit="volume">65</biblScope>
<biblScope unit="issue">1–3</biblScope>
<biblScope unit="page" from="107">107</biblScope>
<biblScope unit="page" to="115">115</biblScope>
</imprint>
<idno type="ISSN">0924-0136</idno>
</series>
<idno type="istex">040A787A1B603C71251632AF6F84F5D0445A9532</idno>
<idno type="DOI">10.1016/0924-0136(95)02249-X</idno>
<idno type="PII">0924-0136(95)02249-X</idno>
</biblStruct>
</sourceDesc>
<seriesStmt>
<idno type="ISSN">0924-0136</idno>
</seriesStmt>
</fileDesc>
<profileDesc>
<textClass></textClass>
<langUsage>
<language ident="en">en</language>
</langUsage>
</profileDesc>
</teiHeader>
<front>
<div type="abstract" xml:lang="en">The deformation characteristics of as-cast 304 stainless steel under compression in the temperature range 20–600 °C and strain rate range 0.001–100 s−1 have been studied with a view to characterizing the flow instabilities occurring in the microstructure. At strain rates of less than 0.05 s−1, as-cast 304 stainless steel exhibits flow localization in the temperature range 20–600 °C, whereas dynamic strain ageing occurs at intermediate temperatures and below 5 s−1. At room temperatures and strain rates of less than 0.05 s−1, martensite formation is observed. To avoid the above microstructural instabilities warm working should be carried out at strain rates greater than 10 s−1 in the temperature range 400–600 °C and cold working could be done in the range of about 0.05–0.8 s−1. The continuum criterion developed on the basis of the principles of maximum rate of entropy production and separability of the dissipation function, predicts accurately all of the above instability features.</div>
</front>
</TEI>
<affiliations>
<list>
<country>
<li>Inde</li>
<li>États-Unis</li>
</country>
<region>
<li>Ohio</li>
</region>
</list>
<tree>
<country name="Inde">
<noRegion>
<name sortKey="Venugopal, S" sort="Venugopal, S" uniqKey="Venugopal S" first="S." last="Venugopal">S. Venugopal</name>
</noRegion>
<name sortKey="Mannan, S L" sort="Mannan, S L" uniqKey="Mannan S" first="S. L." last="Mannan">S. L. Mannan</name>
<name sortKey="Prasad, Y V R K" sort="Prasad, Y V R K" uniqKey="Prasad Y" first="Y. V. R. K." last="Prasad">Y. V. R. K. Prasad</name>
</country>
<country name="États-Unis">
<region name="Ohio">
<name sortKey="Venugopal, S" sort="Venugopal, S" uniqKey="Venugopal S" first="S." last="Venugopal">S. Venugopal</name>
</region>
</country>
</tree>
</affiliations>
</record>

Pour manipuler ce document sous Unix (Dilib)

EXPLOR_STEP=$WICRI_ROOT/Ticri/CIDE/explor/OcrV1/Data/Main/Exploration
HfdSelect -h $EXPLOR_STEP/biblio.hfd -nk 002403 | SxmlIndent | more

Ou

HfdSelect -h $EXPLOR_AREA/Data/Main/Exploration/biblio.hfd -nk 002403 | SxmlIndent | more

Pour mettre un lien sur cette page dans le réseau Wicri

{{Explor lien
   |wiki=    Ticri/CIDE
   |area=    OcrV1
   |flux=    Main
   |étape=   Exploration
   |type=    RBID
   |clé=     ISTEX:040A787A1B603C71251632AF6F84F5D0445A9532
   |texte=   Instability map for cold and warm working of as-cast 304 stainless steel
}}

Wicri

This area was generated with Dilib version V0.6.32.
Data generation: Sat Nov 11 16:53:45 2017. Site generation: Mon Mar 11 23:15:16 2024