Interfacial kinetics of hydrogen with liquid slag containing iron oxide

Identifieur interne : 001946 ( Main/Exploration ); précédent : 001945; suivant : 001947

Interfacial kinetics of hydrogen with liquid slag containing iron oxide

Auteurs : Tetsuya Nagasaka [Japon] ; Mitsutaka Hino [Japon] ; Shiro Ban-Ya [Japon]

Source :

RBID : ISTEX:1D92253F4867852F41745B4B3FA8713C4BD89595

Abstract

Abstract: Interfacial kinetics on the hydrogen reduction of liquid Fe t O in Fe t O-M x O y slag (M x O y = CaO, SiO2, Al2O3, and TiO2) has been studied at 1673 K. Because the rate of hydrogen reduction was very fast, the rate was controlled by gas-phase mass transfer under most of the experimental conditions. The effect of CaO or SiO2 addition on the interfacial chemical reaction rate of hydrogen reduction was empirically evaluated as a function of the ferrous-ferric ratio in the slag. The observed interfacial chemical reaction rates in Fe t O-CaO and Fe t O-SiO2 slags showed reasonable agreement with the estimated values. Most of the available literature data on the reduction rate of liquid iron oxide by solid carbon, hot metal, and reducing gases were also reviewed and compared with the results of the present work. It was found that the rate of hydrogen reduction of liquid iron oxide slag is much faster than that with other reducing agents such as solid carbon, carbon dissolved in the liquid iron, and CO gas.

Url:
DOI: 10.1007/s11663-000-0071-6


Affiliations:


Links toward previous steps (curation, corpus...)


Le document en format XML

<record>
<TEI wicri:istexFullTextTei="biblStruct">
<teiHeader>
<fileDesc>
<titleStmt>
<title xml:lang="en">Interfacial kinetics of hydrogen with liquid slag containing iron oxide</title>
<author>
<name sortKey="Nagasaka, Tetsuya" sort="Nagasaka, Tetsuya" uniqKey="Nagasaka T" first="Tetsuya" last="Nagasaka">Tetsuya Nagasaka</name>
</author>
<author>
<name sortKey="Hino, Mitsutaka" sort="Hino, Mitsutaka" uniqKey="Hino M" first="Mitsutaka" last="Hino">Mitsutaka Hino</name>
</author>
<author>
<name sortKey="Ban Ya, Shiro" sort="Ban Ya, Shiro" uniqKey="Ban Ya S" first="Shiro" last="Ban-Ya">Shiro Ban-Ya</name>
</author>
</titleStmt>
<publicationStmt>
<idno type="wicri:source">ISTEX</idno>
<idno type="RBID">ISTEX:1D92253F4867852F41745B4B3FA8713C4BD89595</idno>
<date when="2000" year="2000">2000</date>
<idno type="doi">10.1007/s11663-000-0071-6</idno>
<idno type="url">https://api.istex.fr/ark:/67375/VQC-34Q7GCTM-X/fulltext.pdf</idno>
<idno type="wicri:Area/Istex/Corpus">001500</idno>
<idno type="wicri:explorRef" wicri:stream="Istex" wicri:step="Corpus" wicri:corpus="ISTEX">001500</idno>
<idno type="wicri:Area/Istex/Curation">001500</idno>
<idno type="wicri:Area/Istex/Checkpoint">000761</idno>
<idno type="wicri:explorRef" wicri:stream="Istex" wicri:step="Checkpoint">000761</idno>
<idno type="wicri:doubleKey">1073-5615:2000:Nagasaka T:interfacial:kinetics:of</idno>
<idno type="wicri:Area/Main/Merge">001989</idno>
<idno type="wicri:Area/Main/Curation">001946</idno>
<idno type="wicri:Area/Main/Exploration">001946</idno>
</publicationStmt>
<sourceDesc>
<biblStruct>
<analytic>
<title level="a" type="main" xml:lang="en">Interfacial kinetics of hydrogen with liquid slag containing iron oxide</title>
<author>
<name sortKey="Nagasaka, Tetsuya" sort="Nagasaka, Tetsuya" uniqKey="Nagasaka T" first="Tetsuya" last="Nagasaka">Tetsuya Nagasaka</name>
<affiliation wicri:level="4">
<country xml:lang="fr">Japon</country>
<wicri:regionArea>the Department of Metallurgy, Graduate School of Engineering, Tohoku University, 980-8579, Sendai</wicri:regionArea>
<orgName type="university">Université du Tōhoku</orgName>
<placeName>
<settlement type="city">Sendai</settlement>
<region type="province">Région de Tōhoku</region>
</placeName>
</affiliation>
</author>
<author>
<name sortKey="Hino, Mitsutaka" sort="Hino, Mitsutaka" uniqKey="Hino M" first="Mitsutaka" last="Hino">Mitsutaka Hino</name>
<affiliation wicri:level="4">
<country xml:lang="fr">Japon</country>
<wicri:regionArea>the Department of Metallurgy, Graduate School of Engineering, Tohoku University, 980-8579, Sendai</wicri:regionArea>
<orgName type="university">Université du Tōhoku</orgName>
<placeName>
<settlement type="city">Sendai</settlement>
<region type="province">Région de Tōhoku</region>
</placeName>
</affiliation>
</author>
<author>
<name sortKey="Ban Ya, Shiro" sort="Ban Ya, Shiro" uniqKey="Ban Ya S" first="Shiro" last="Ban-Ya">Shiro Ban-Ya</name>
<affiliation wicri:level="1">
<country xml:lang="fr">Japon</country>
<wicri:regionArea>Iohoku University and Akita National College of Technology</wicri:regionArea>
</affiliation>
</author>
</analytic>
<monogr></monogr>
<series>
<title level="j">Metallurgical and Materials Transactions B</title>
<title level="j" type="abbrev">Metall and Materi Trans B</title>
<idno type="ISSN">1073-5615</idno>
<idno type="eISSN">1543-1916</idno>
<imprint>
<publisher>Springer-Verlag</publisher>
<pubPlace>New York</pubPlace>
<date type="published" when="2000-10-01">2000-10-01</date>
<biblScope unit="volume">31</biblScope>
<biblScope unit="issue">5</biblScope>
<biblScope unit="page" from="945">945</biblScope>
<biblScope unit="page" to="955">955</biblScope>
</imprint>
<idno type="ISSN">1073-5615</idno>
</series>
</biblStruct>
</sourceDesc>
<seriesStmt>
<idno type="ISSN">1073-5615</idno>
</seriesStmt>
</fileDesc>
<profileDesc>
<textClass></textClass>
<langUsage>
<language ident="en">en</language>
</langUsage>
</profileDesc>
</teiHeader>
<front>
<div type="abstract" xml:lang="en">Abstract: Interfacial kinetics on the hydrogen reduction of liquid Fe t O in Fe t O-M x O y slag (M x O y = CaO, SiO2, Al2O3, and TiO2) has been studied at 1673 K. Because the rate of hydrogen reduction was very fast, the rate was controlled by gas-phase mass transfer under most of the experimental conditions. The effect of CaO or SiO2 addition on the interfacial chemical reaction rate of hydrogen reduction was empirically evaluated as a function of the ferrous-ferric ratio in the slag. The observed interfacial chemical reaction rates in Fe t O-CaO and Fe t O-SiO2 slags showed reasonable agreement with the estimated values. Most of the available literature data on the reduction rate of liquid iron oxide by solid carbon, hot metal, and reducing gases were also reviewed and compared with the results of the present work. It was found that the rate of hydrogen reduction of liquid iron oxide slag is much faster than that with other reducing agents such as solid carbon, carbon dissolved in the liquid iron, and CO gas.</div>
</front>
</TEI>
<affiliations>
<list>
<country>
<li>Japon</li>
</country>
<region>
<li>Région de Tōhoku</li>
</region>
<settlement>
<li>Sendai</li>
</settlement>
<orgName>
<li>Université du Tōhoku</li>
</orgName>
</list>
<tree>
<country name="Japon">
<region name="Région de Tōhoku">
<name sortKey="Nagasaka, Tetsuya" sort="Nagasaka, Tetsuya" uniqKey="Nagasaka T" first="Tetsuya" last="Nagasaka">Tetsuya Nagasaka</name>
</region>
<name sortKey="Ban Ya, Shiro" sort="Ban Ya, Shiro" uniqKey="Ban Ya S" first="Shiro" last="Ban-Ya">Shiro Ban-Ya</name>
<name sortKey="Hino, Mitsutaka" sort="Hino, Mitsutaka" uniqKey="Hino M" first="Mitsutaka" last="Hino">Mitsutaka Hino</name>
</country>
</tree>
</affiliations>
</record>

Pour manipuler ce document sous Unix (Dilib)

EXPLOR_STEP=$WICRI_ROOT/Sante/explor/H2N2V1/Data/Main/Exploration
HfdSelect -h $EXPLOR_STEP/biblio.hfd -nk 001946 | SxmlIndent | more

Ou

HfdSelect -h $EXPLOR_AREA/Data/Main/Exploration/biblio.hfd -nk 001946 | SxmlIndent | more

Pour mettre un lien sur cette page dans le réseau Wicri

{{Explor lien
   |wiki=    Sante
   |area=    H2N2V1
   |flux=    Main
   |étape=   Exploration
   |type=    RBID
   |clé=     ISTEX:1D92253F4867852F41745B4B3FA8713C4BD89595
   |texte=   Interfacial kinetics of hydrogen with liquid slag containing iron oxide
}}

Wicri

This area was generated with Dilib version V0.6.33.
Data generation: Tue Apr 14 19:59:40 2020. Site generation: Thu Mar 25 15:38:26 2021